Scratches on Matt Surface
STEP 1
Remove all loose and splintered particles.
Use the Edge Planer to press damage edges slightly down to obtain smooth transitions.
Products required:
STEP 2
STEP 3
Strip off projectings in still heated condition evenly with the leading edge of the Special Filler Applicator or after cooling down (approx. 1 min.) with the Metal Planer.
STEP 4
Make an intermediate sealing by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.
Replicate grain using the Graining Pen.
STEP 5
Products required:
STEP 6
Use Special Repair Lacquer to seal and to protect repaired area from dust and dirt and to adjust the sheen level, if necessary.
Alternatively, you can also use the Brush-Fix Clear Pen for sealing and sheen level adjustment.