Laminate Abrasions

STEP 1

Clean the surface.

Products required:

STEP 2

Make an intermediate sealing by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.

Products required:

STEP 3

Choose several color shades of Brush-Fix Pigment Pens corresponding to the surface and color abrasions in the basic shade.

Products required:

STEP 4

Restore the grain using the Graining Pen.

Products required:

STEP 5

Seal retouched area by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.