Laminate Abrasions
Browse:
STEP 1
STEP 2
![](https://alliedpianoandfinish.com/wp-content/uploads/Laminate-Abrasions-Step-2.jpg)
Make an intermediate sealing by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.
Products required:
STEP 3
![](https://alliedpianoandfinish.com/wp-content/uploads/Laminate-Abrasions-Step-3.jpg)
Choose several color shades of Brush-Fix Pigment Pens corresponding to the surface and color abrasions in the basic shade.
Products required:
STEP 4
STEP 5
![](https://alliedpianoandfinish.com/wp-content/uploads/Laminate-Abrasions-Step-5.jpg)
Seal retouched area by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.
Products required: