Laminate Abrasions

Browse:

STEP 1

Tips Laminate Abrasions

Clean the surface.

Products required:

STEP 2

Laminate Abrasions Step 2
Make an intermediate sealing by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.

Products required:

STEP 3

Laminate Abrasions Step 3

Choose several color shades of Brush-Fix Pigment Pens corresponding to the surface and color abrasions in the basic shade.

Products required:

STEP 4

Laminate Abrasions Step 4
Restore the grain using the Graining Pen.

Products required:

STEP 5

Laminate Abrasions Step 5
Seal retouched area by misting with Special Repair Lacquer from a distance of 12-16 inches – do not spray too wet.